I probably should have mentioned in my last post, you don't need to start from scratch.  Here are a few of the standard sizes that we have just waiting to string your cells:

 

2 mm wide x 0.10 mm thick

2 mm wide x 0.15 mm thick

1.5 mm wide x 0.10 mm thick

1.5 mm wide x 0.15 mm thick

5.0 mm wide x 0.40 mm thick

 

Standard alloy coatings include: 

 

Sn96, 96.5% tin, 3.5% silver

SN60, 60% tin, 40% lead

SN62, 60% tin, 38% lead, 2% silver