From One Engineer to Another

Liquid Metal Wetting

Monday, April 6, 2009 by Jim Hisert [Jim Hisert]

I assure you, the following is not some strange alien test of foreign materials. Even though it resembles a substance from the spaceship in E.T. – this is definitely earthly matter. This video shows the following 3 low-temperature liquid metal alloys wetting to glass:

  • 61Ga/25In/13Sn/1Zn (Indalloy #46L)
  • 66.5Ga/20.5In/13Sn
  • 68.5Ga/21.5In/10Sn

These are variations of Gallium, Indium, and Tin (with Zinc in #46L) that have amazing abilities – including incredibly low thermal resistance in heat transfer applications. These alloys also wet to other non-metallic substrates like silicon, quartz, ceramics, and diamond.

 

Call us @ (315) 853-4900, or email us if you'd like to learn more about metals that are liquid at room temperature.