A passage from Metals Handbook, Volume 6, 1983Ӕ
Fact: To achieve a strong, reliable solder joint, it is important to remove all oxides from the substrate as well as the solder. Generally this is done using a compatible flux.
Reality: Sometimes flux cannot be used, so it is important that the starting materials be as oxide-free as possible. Au/Sn is a popular solder in flux-less applications. The preform is a popular form for Au/Sn because it delivers a consistent, controlled amount of solder every time. However, unless properly controlled, the manufacturing process can introduce oxides that become imbedded in the material and cannot be easily cleaned.
Solution: Indium Corporation has perfected its process used to manufacture Au/Sn preforms. This is no small task. Our experienced Metallurgists and Process Engineers have taken a good thing and made it even better. If you're looking for proof, talk with one of our Application Engineers about evaluating Indium Corp. Au/Sn preforms in your process!