Indium Corporation
From One Engineer to Another®

Tin Whiskers Found in Toyota Brake Assemblies

Tuesday, September 6, 2011 by Dr. Ron Lasky [Dr. Ron Lasky]

Folks,

You may remember that more than a year ago there was much speculation that tin whiskers may be behind the Toyota unintended acceleration problem. At the time I spoke out because there was no data to support the speculation. Now there is data, Mike Pecht and his CALCE Team at the University of Maryland, found numerous tin whiskers in the Toyota brake assemblies of concern.

Although the tin whiskers were not implicated in any failure, their presence is cause for alarm, and action should be taken to address this issue. Tin whiskers should not be found in mission critical devices. Pecht’s team has an algorithm that calculates the risk from tin whiskers that are discovered. The risk is 140 per 1 million not high, but with a million or so Toyotas on the road, clearly this is cause for alarm.

BethelAs you may know, I live in Woodstock, Vermont.  Many friends have asked how we are doing after hurricane Irene. Personally, my wife and I escaped with no damage to our house and only a bit of inconvenience (no water for 5 days). The town of Woodstock suffered considerable damage, but was, on the whole, fortunate. Some of the neighboring towns had all roads in and out washed away. Route 4 between Woodstock and Rutland has numerous sections destroyed. The flooding was declared by the governor to be the worst disaster in Vermont history. The photo is from the Valley News. It shows a wooden pedestrian bridge built to carry supplies into Bethel, VT by foot. There is no passable road, even for ATVs.

Best,

Dr. Ron

Comments for Tin Whiskers Found in Toyota Brake Assemblies

Sunday, November 6, 2011 by retep497:
CACLE team foun tin whiskers in the accelerator pedal (not the brake assembly). Also, NASA has found tin whiskers last year during its investigation of Toyota's electronics and software but didn't make a big issue out of it even though such a resisitive short won't be logged by the computer and can cause unitended acceleration. Prof Gilbert also demonstrated that a resistive short can cause unitended acceleration that won't trigger an error code..It seems that in addition to the floor mat issue, the "sticky pedal" issue and the driver error issue, the tin whisker is a more serious and far less understood problem in the automative industry.