Click on the Table of Scpecialty Alloys link on the Indium homepage to view physical properties of more than 200 alloys used for their thermal and mechanical properties.

Click on the Table of Scpecialty Alloys link on the Indium homepage to view physical properties of more than 200 alloys used for their thermal and mechanical properties.

When I need any information on a direct attach solder thermal interface material, my first line of defense is my solder alloy directory, also known as the "Table of Specialty Alloys and Solders". 

 

The information in this literature is available to you as well on Indiums website.҂ It contains the most popular as well as the unusually-requested solders along with many of their physical properties. Over 200 solder alloys are listed (all of which could be used as a thermal interface material) and at a minimum, you will find the melting temperatures of these materials. For many of the materials, thermal, electrical, and physical properties of each alloy are also listed.